01 / DRI · Largest Vertical
Sponge Iron
Our largest product line. Direct Reduced Iron (DRI) sourced from primary producers across Chhattisgarh, Odisha, West Bengal & Jharkhand, supplied in three forms for steel plant and induction furnace charge mix.
Sponge Iron Pellets
| Parameter | Typical Value |
| Fe (Total) | 78% ± 1 |
| Fe (Metallic) | 65% – 70% |
| Metallization | 82% – 88% |
| Carbon (C) | 0.10% – 0.20% |
| Sulphur (S) | 0.02% – 0.03% max |
| Phosphorus (P) | 0.03% – 0.05% max |
| Gangue (SiO2 + Al2O3) | 3% – 5% |
| Size | 5mm – 18mm |
Sponge Iron Lumps
| Parameter | Typical Value |
| Fe (Total) | 79% ± 1 |
| Fe (Metallic) | 66% – 71% |
| Metallization | 83% – 89% |
| Carbon (C) | 0.10% – 0.20% |
| Sulphur (S) | 0.02% – 0.03% max |
| Phosphorus (P) | 0.03% – 0.05% max |
| Gangue (SiO2 + Al2O3) | 3% – 5% |
| Size | 3mm – 18mm |
Sponge Iron Fines
| Parameter | Typical Value |
| Fe (Total) | 79% ± 1 |
| Fe (Metallic) | 66% – 71% |
| Metallization | 83% – 89% |
| Carbon (C) | 0.10% – 0.20% |
| Sulphur (S) | 0.02% – 0.03% max |
| Phosphorus (P) | 0.03% – 0.05% max |
| Gangue (SiO2 + Al2O3) | 3% – 5% |
| Size | Below 3mm |
Note: Fe% for pellets, lumps and fines are set from your figures. Metallization, carbon, sulphur, phosphorus and gangue are typical DRI industry ranges, not assayed numbers. Send actual lab reports to lock these tables to your product.
Cast billet ingots for re-rolling into structural steel, coarser as-cast grain structure than continuously cast billets.
| Element | Typical Composition |
| Carbon (C) | 0.15% – 0.25% |
| Manganese (Mn) | 0.50% – 0.80% |
| Silicon (Si) | 0.15% – 0.35% |
| Sulphur (S) | 0.055% max |
| Phosphorus (P) | 0.055% max |
| Combined S + P | 0.11% max |
Note: figures reflect standard IS 2830/2831 ranges. Send your typical ladle analysis if you want this locked to your actual trading grade.
Continuously cast billets with a more uniform grain structure and fewer internal defects than cast ingots, preferred by modern rolling mills.
| Element | Typical Composition |
| Carbon (C) | 0.15% – 0.25% |
| Manganese (Mn) | 0.50% – 0.80% |
| Silicon (Si) | 0.15% – 0.35% |
| Sulphur (S) | 0.050% max |
| Phosphorus (P) | 0.050% max |
| Tensile Strength | 400 – 550 MPa (grade dependent) |
Note: figures reflect standard trade ranges. Send your typical size and chemistry if you want this locked to your actual trading grade.
04 / Ferroalloy
Silico Manganese (SiMn)
Ferroalloy used as a deoxidizer and alloying element in steel production, supplied to induction furnaces, EAFs and steel plants.
| Grade | Mn % | Si % | C % max | P % max | S % max |
| SiMn 60/14 (standard) | 60 – 65 | 14 – 17 | 2.5 | 0.30 | 0.03 |
| SiMn 65/16 (high grade) | 65 – 70 | 16 – 20 | 2.0 | 0.30 | 0.03 |
| Low carbon variants | 65 – 74 | 16 – 20 | 1.0 – 1.5 | 0.20 – 0.30 | 0.02 – 0.05 |
Note: table reflects standard industry grades aligned with IS 1470. Confirm which grade(s) you trade so this matches your actual product.
Imported steam coal across three origins, sourced at the Kandla, Tuna, Mundra and Navlakhi ports in Gujarat, graded by GCV and delivered to industries across North India by rail and road.
| Origin | Typical Grade | Use Cases |
| USA (NAPP) | High GCV, ~6900 NAR / 7200 Kcal/Kg | Steel plants, cement kilns, high heat boilers |
| USA (ILB) | ~6500 Kcal/Kg, higher sulphur | Brick kilns, steel plants, industrial fuel |
| Indonesian | ~4200 GAR (commonly traded) | Brick kilns, thermal and boiler applications |
| Russian | High sulphur, high performance | Power utilities, steel plants, thermal generation |
Note: figures are indicative industry standard grades from public data. Confirm your exact GCV/sizing specs so we can lock in accurate numbers.